AT Plastics AT Plastics AT 192 Low Density Polyethylene (LDPE)
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: carpet extrusion coating applications
Material Notes: AT 192 is a homopolymer that is suitable for use in carpet extrusion coating applications. This polymer may be processed on conventional extrusion coating equipment. Additives: Applications: Automotive
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|