INEOS ABS Centrex® 825 ASA+AES Blend
Subcategory: AES Polymer; ASA Polymer; Thermoplastic
Close Analogs: LANXESS was spun-off from Bayer in early 2005.
Material Notes: Key Features:- Unfilled
- High impact or high impact modified
- Light stabilized or stable to light
- U.V. stabilized or stable to weather
Suitable processing methods: - Profile extrusion
- Sheet extrusion
- Thermoforming
Information provided by Bayer Polymers.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Dissipation Factor
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Injection Velocity
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|