LANXESS Durethan® KU 2-2036/30 HTS Nylon 6 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Close Analogs: LANXESS was spun-off from Bayer in early 2005. This product is no longer listed as a standard NAFTA product.
Key Words: Polyamide 6
Material Notes: Key Features:- Contains Filler
- Heat stabilized or stable to heat
Suitable processing methods: Information provided by Bayer Polymers.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 8.0 MPa
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Melt Temperature
- Mold Temperature
- Injection Velocity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|