LANXESS Durethan® T40 ZS Copolyamide 66/6T (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 66; Nylon 6
Close Analogs: LANXESS was spun-off from Bayer in early 2005.
Material Notes: Key Features: Suitable processing methods: - Injection molding
- Film extrusion
- Profile extrusion
Information provided by Bayer Polymers.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Transmission, Visible
- Melt Temperature
- Mold Temperature
- Injection Velocity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|