Bayer MaterialScience Makroblend® EL-700 Polycarbonate + Polyester Blend
Subcategory: Polycarbonate; Polyester, TP; Thermoplastic
Material Notes: Key Features:- Flame retarding agent
- Unfilled
- High impact or high impact modified
- Light stabilized or stable to light
Suitable processing methods: Information provided by Bayer Polymers.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Injection Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|