Bayer MaterialScience Texin® 285 Urethane Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Key Features: Suitable processing methods: - Injection molding
- Film extrusion
- Profile extrusion
- Sheet extrusion
- Coating
- Blow molding
Information provided by Bayer Polymers.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Vicat Softening Point
- Glass Temperature
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Injection Pressure
|
|
|
|