Bayer MaterialScience Texin® 985U Urethane Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Key Words: TPU
Material Notes: Key Features:- Unfilled
- U.V. stabilized or stable to weather
Suitable processing methods: - Injection molding
- Film extrusion
- Profile extrusion
- Sheet extrusion
- Blow molding
Information provided by Bayer Polymers.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Vicat Softening Point
- Glass Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
|
|
|
|