Bayer MaterialScience Bayblend® SF 1443 Polycarbonate + ABS Blend Structural Foam
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic
Key Words: PC+ABS; Poly(Acrylonitrile Butadiene Styrene)
Material Notes: Foam thickness 0.250 in. Properties values at foam density of 0.90 g/cc. Information provided by Bayer Corporation, Plastics Division
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|