INEOS ABS Centrex® 401 AES, Extrusion
Subcategory: AES Polymer; Thermoplastic
Close Analogs: LANXESS was spun-off from Bayer in early 2005. This product is no longer listed as a standard NAFTA product.
Material Notes: Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with <10% orientation. Information provided by Bayer Corporation, Plastics Division
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Impact Test
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Gloss
- Transmission, Visible
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|