Bayer MaterialScience Baydur® 726 IBS, Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System
Subcategory: Polyurethane, TS; Thermoset; Composite Core Material
Material Notes: 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection Molding Information provided by Bayer Corporation, Polyurethanes Division
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Charpy Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|