Bayer MaterialScience Baydur® STR/C-400 BB, Polyurethane Composite SRIM Foam, 60% Glass Filled, MDI-based 2-Component Liquid System
Subcategory: Polyurethane, TS; Thermoset; Polymer
Material Notes: Contains directed chopped fiber preform glass. 0.16 in. thickness. Information provided by Bayer Corporation, Polyurethanes Division
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |