Bayer MaterialScience Baydur® STR/C-405 IMR, Polyurethane Composite SRIM Foam, 45% Glass Filled, MDI-based 2-Component Liquid System
Subcategory: Polyurethane, TS; Thermoset; Polymer
Material Notes: Contains continuous strand fiberglass mat. 0.118 in. thickness. Information provided by Bayer Corporation, Polyurethanes Division
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|