LANXESS DURETHAN® A 30 Nylon 66, Injection Grade, Dry As Molded
Subcategory: Nylon; Thermoplastic; Nylon 66
Close Analogs: LANXESS was spun-off from Bayer in early 2005. See separate entry for conditioned properties.
Key Words: Nylon 6/6; Polyamide 66
Material Notes: Standard injection molding grade, easy mold release, normal setting, isotropic shrinkage. Applications: Electrical sector: terminal blocks, cable ties, housing parts, coil bodies, transformer housings. Other: gear wheels. Information provided by Bayer.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|