LANXESS DURETHAN® A 31 SK Nylon 66, Injection Grade, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 66
Close Analogs: LANXESS was spun-off from Bayer in early 2005. See separate entry for dry as molded properties.
Key Words: Nylon 6/6; Polyamide 66
Material Notes: Standard injection molding grade, swiftly setting, with feeding aid, only available in natural or with color concentrate. Applications: Electrical sector: terminal blocks, cable ties, housing parts, coil bodies, transformer housings. Information provided by Bayer.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|