LANXESS DURETHAN® BKV 30 H1.0/H2.0 Nylon 6, 30% Glass Fiber, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Close Analogs: LANXESS was spun-off from Bayer in early 2005. See separate entry for dry as molded properties.
Key Words: Polyamide 6; PA6
Material Notes: Injection molding grade with 30% glass fibers, heat stabilized. Applications: Automotive sector: cooling fans, gears for tachometer drive, door handles, tractor bonnet, air inlet manifolds. Electrical sector: fan wheel for ventilator Information provided by Bayer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|