LANXESS DURETHAN® KU 2-2235/30 H1.0 Nylon 66, 30% Glass Fiber, As Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Close Analogs: LANXESS was spun-off from Bayer in early 2005. See separate entry for dry as molded properties.
Key Words: Nylon 6/6; Polyamide 66; PA66
Material Notes: Injection molding grade with 30% glass fibers, elastomer modified, heat stabilized (also available in H2.0). Applications: Automotive sector: airbag housings, pedals. Information provided by Bayer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Modulus
- Flammability, UL94
|
|
|
|