INEOS ABS Novodur® ABS 348
Subcategory: ABS Polymer; Thermoplastic
Close Analogs: LANXESS was spun-off from Bayer in early 2005.
Key Words: Poly(Acrylonitrile-Butadiene-Styrene)
Material Notes: Special grade for medical applications, biocompatible. Information provided by Bayer.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Charpy Impact, Notched
- Impact Test
- Electrical Resistivity
- Surface Resistance
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|