LANXESS POCAN® KU 2-7018 PBT, Extrusion Grade
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Close Analogs: LANXESS was spun-off from Bayer in early 2005.
Key Words: Polyester; Polybutylene Terephthalate
Material Notes: PBT-extrusion grade, non-reinforced, high viscosity, elastomer modified. Applications: Other: top layers for skis. Information provided by Bayer.