INEOS ABS Triax® 1220 S ABS/Nylon Blend, Dry as Molded
Subcategory: Nylon; ABS Polymer; Thermoplastic
Close Analogs: LANXESS was spun-off from Bayer in early 2005. See separate entry for conditioned properties.
Key Words: Polyamide; Poly(Acrylonitrile-Butadiene-Styrene)
Material Notes: Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping behavior. Information provided by Bayer.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|