Hexion PF 13 Phenolic Formaldehyde Resin, UL Listed
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Bakelite AG has become Hexion Specialty Chemicals GmbH in 2005. The status of this product is unknown.
Material Notes: Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound. Application areas: Electric motor slip ring commutators, commutators (adjustment motors, truck starter motors, vacuum cleaners, kitchen devices, electrical tools, electrical vehicles), bobbins. Information provided by Bakelite AG
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Ball Indentation Hardness
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- High Voltage Arc Resistance to Ignition (HVAR)
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- Maximum Service Temperature, Air
- Deflection Temperature at 8.0 MPa
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Shrinkage
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
- Back Pressure
- Cure Time
- Chromatic Spectrum
- Creep Rupture Strength
- Holding Pressure
- Media Resistance
- Moisture Absorption
- Reserves by Peak Temperature
- Thermal Expansion
|
|
|
|
| Property Data |
This page displays only the text