Hexion PF 4155 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Bakelite AG has become Hexion Specialty Chemicals GmbH in 2005. The status of this product is unknown.
Material Notes: Phenolic molding compound, inorganically filled, glass fiber reinforced, good media and temperature resistance. Conditioned Cu-adhesion. Application areas: Commutators (fuel pumps, actuators, starter motors, HVAC motors, fan motors, window lift motors, ABS, wiper motors, garden appliances, household appliances, power tools, universal motors). Information provided by Bakelite AG
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Ball Indentation Hardness
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 8.0 MPa
- Shrinkage
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
- Back Pressure
- Cure Time
- Chromatic Spectrum
- Creep Rupture Strength
- Holding Pressure
- Media Resistance
- Moisture Absorption
- Reserves by Peak Temperature
- Thermal Expansion
|
|
|
|
| Property Data |
This page displays only the text