Hexion PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Bakelite AG has become Hexion Specialty Chemicals GmbH in 2005. The status of this product is unknown.
Material Notes: Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength. Application areas: Moldings for higher mechanical strain, e.g. power plugs high voltage, handles, knobs. Information provided by Bakelite AG
| Available Properties |
- Density
- Linear Mold Shrinkage
- Ball Indentation Hardness
- Tensile Strength at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 8.0 MPa
- Shrinkage
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
- Back Pressure
- Cure Time
- Chromatic Spectrum
- Creep Rupture Strength
- Holding Pressure
- Media Resistance
- Moisture Absorption
- Reserves by Peak Temperature
- Thermal Expansion
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|