Hexion UP 3620 Unsaturated Polyester Resin, High Surface Quality, UL Listed
Subcategory: Polyester, TS; Thermoset; Polymer
Close Analogs: Bakelite AG has become Hexion Specialty Chemicals GmbH in 2005. The status of this product is unknown.
Material Notes: Polyester molding compound, mainly organically filled, styrene free, processing shrinkage as for phenolic molding compounds, non flammable, high surface quality, UL listed molding compound 1.5 mm/V-0 (ALL). Application areas: Lamp housings, neon tube end parts and bases, switch gears, watt hour meter housings and base plates. Information provided by Bakelite AG
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Ball Indentation Hardness
- Tensile Strength at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- High Voltage Arc Resistance to Ignition (HVAR)
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- Maximum Service Temperature, Air
- Deflection Temperature at 8.0 MPa
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Shrinkage
- Feed Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
- Back Pressure
- Cure Time
- Creep Rupture Strength
- Holding Pressure
- Media Resistance
- Moisture Absorption
- Reserves by Peak Temperature
- Thermal Expansion
|
|
|
|
| Property Data |
This page displays only the text