Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8"
Subcategory: Polyester, TS; Thermoset; Polymer
Key Words: Fiber Reinforced Plastic (FRP)
Material Notes: Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:- High Strength
- Corrosion Resistant to many chemicals
- Light Weight- Weighs nearly 80% less than a steel profile of similar dimension
- Electrically Non-Conductive
- Non-Metallic
- Lower Life Cycle Cost
- Non-Leaching. Environmentally Friendly
- Dimensional Stability
Information provided by Bedford Plastics.
| Available Properties |
- Density
- Water Absorption
- Hardness, Barcol
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Compressive Modulus
- Ultimate Bearing Strength
- Shear Strength
- Izod Impact, Notched
- Dielectric Strength
- Dielectric Strength
- Arc Resistance
- CTE, linear 20°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|