Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/16" to 1/4"

 

Subcategory: Polyester, TS; Thermoset; Polymer

Key Words: Fiber Reinforced Plastic (FRP)

Material Notes:
Flame retardant grade; see details in the property table.

Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:

  • High Strength
  • Corrosion Resistant to many chemicals
  • Light Weight- Weighs nearly 80% less than a steel profile of similar dimension
  • Electrically Non-Conductive
  • Non-Metallic
  • Lower Life Cycle Cost
  • Non-Leaching. Environmentally Friendly
  • Dimensional Stability

Information provided by Bedford Plastics.

Available Properties
  • Density
  • Water Absorption
  • Hardness, Barcol
  • Tensile Strength, Ultimate
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • Compressive Modulus
  • Ultimate Bearing Strength
  • Shear Strength
  • Izod Impact, Notched
  • Dielectric Strength
  • Dielectric Strength
  • Arc Resistance
  • CTE, linear 20°C
  • Flammability, UL94
  • Flame Spread Index
  • NBS Smoke Density
  • Flammability
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。