Bhansali Abstron ABS AN-450 EVM Flame Retardent ABS Grade
Subcategory: ABS Polymer; Thermoplastic
Material Notes: ABS-Polycarbonate alloy with Flame Retardancy, general purpose FR-ABS and Sheet Extrusion Grade with FR feature conforming to UL 94 V0 and V2 specifications. Some of the grades are UL certifiedInformation provided by Bhansali
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength @ Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|