Bionate® Polycarbonate-Urethane (PCU), 80 Shore A
Subcategory: Polycarbonate; Polyurethane, TP; Thermoplastic
Key Words: The Polymer Technology Group; Polyurethane; PCU
Material Notes: Clear to slightly cloudy appearance. Molecular Weight Average (GPC) is 264,000; Molecular Weight Number (GPC) is 81,000. Polydispersity (Mw/Mn) is 3.2. Recommended sterilization method is ethylene oxide. Passes USP XXII Class VI Biological Reaction. Bionate® PCUs were formerly manufactured under the tradename Corethane® Polycarbonate Urethanes by Corvita Corp. The patented Corethane/Coremer/Corehesive polymers are among the most extensively tested biomaterials yet developed, and they are the first biomedical polyurethanes to be promoted for their biostability. This family of materials achieves oxidative stability through a replacement of susceptible ether groups with carbonate linkages adjacent to hydrocarbon groups. This makes these polymers attractive in applications in which oxidation is a potential mode of degradation, such as in pacemaker leads. Information provided by The Polymer Technology Group.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- 100% Modulus
- Flexural Modulus
- Flexural Yield Strength
- Coefficient of Friction
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- CTE, linear 20°C
- Vicat Softening Point
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|