Bulk Molding Compounds BMC 100 Thermoset Polyester, GP
Subcategory: Polyester, TS; Thermoset
Material Notes: BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is well suited for injection, transfer or compression molding of intricate parts.Typical applications are circuit breakers, insulators, bobbins and electrical connectors.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|