Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds belongs to this material series. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk and can be customized for specific applications.Typical applications include Sinks, Grill Shelves, and Distributor Caps.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|