Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound
Subcategory: Polyester, TS; Thermoset
Material Notes: BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coating systems and demonstrates excellent adhesion characteristics. BMC 304 can be supplied in logs, slugs or bulk form.Typical applications include Automotive Headlamp and Foglamp Reflectors, and Automotive Body Panels.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|