Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
Subcategory: Polyester, TS; Thermoset
Material Notes: BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|