Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties And extremely low water absorption. This product has a low mold shrinkage and resists the formation of internal voids normally associated with glass filled compounds.Typical applications include slip rings, brush holders and connector bases.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|