Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material with medium impact strength and good overall electrical properties.Typical applications include slip rings, commutators and brush holders.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|