Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good moldability, medium impact strength, excellent overall electrical properties and flame resistance.Typical applications include circuit breakers, transformer bobbins and motor end bells.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|