Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade
Subcategory: Polyester, TS; Thermoset
Material Notes: BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are microwave cookware and airline dishes.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|