Bulk Molding Compounds BMC 1100 Corelyn Glass Fiber Reinforced Polyester Compound
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: BMC 1100, also known as CoreLyn, is a food contact safe material with excellent scratch and stain resistant properties. CoreLyn can be pigmented to match virtually any color. This glass fiber-reinforced polyester compound is suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, Corelyn can be supplied in logs, slugs, or bulk.Typical applications are microwave dishware and serving trays.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|