Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd
Subcategory: Polyester, TS; Thermoset; Polymer
Material Notes: BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better abrasion resistance than that available with other BMC products
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Mold Temperature
|
|
|
|