Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester
Subcategory: Polyester, TS; Thermoset
Material Notes: BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame resistance and electrical characteristics.Typical applications include third rail and other rapid transit insulators.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Track Resistance
- Comparative Tracking Index
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Flammability Test
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|