Bulk Molding Compounds BMC 845 30% Glass Filled Vinyl Ester
Subcategory: Vinyl Ester; Thermoset; Polymer
Material Notes: BMC 845 is designed for use in PEM type fuel cell applications such as end plates and manifolds. It is a corrosion resistant product that shows outstanding creep resistance and compressive creep at elevated temperatures. It can be easily injection compression molded or compression molded depending on the applications requirements. This product is available in bulk and extruded forms.