Borealis Visico™ LE4423/Ambicat™ LE4472 Black, Fast Curing, Silane Crosslinkable LDPE Compound for Weather Resistant Covering/Insulation of Overhead Cables
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. This polyethylene compound is highly active and crosslinks rapidly under ambient temperature and humidity conditions, as well as, in a sauna or hot water bath. The combinations of the Visico base material, LE 4423, and the patented sulphonic acid catalyst masterbatch, LE4472, provides a highly scorch retardant compound with excellent thermal stability. LE4423 contains a permanent scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound, minimizes the tendency for premature crosslinking in the extruder, head or die and allows the use of a highly active crosslinking catalyst like LE4472. LE4472 should be added to LE4423 directly in the extruder hopper by dry blending at a ratio of 7 parts LE4472 to 93 parts LE4423. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Index of Compound
- Deformation
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor, Low Frequency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|