Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets
Subcategory: Polypropylene; Thermoplastic
Material Notes: Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at low temperatures, increased hydrostatic strength and improved chemical resistance.Beta(ß)-PP BE60-7032 is recommended for pressure pipes and fittings, chemical engineering components, extruded and compression molded sheets, filter plates and solid rods. The material is colored grey based on RAL 7032. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Head Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|