Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Subcategory: Polypropylene; Thermoplastic
Material Notes: Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of the excellent performance characteristics of Beta-PPR RA7050-GN is, for example, a categorized required strength (CRS) of 5 MPa at 70°C and 50 years in comparison to a value of 3.21 MPa for standard PP-R. The color of Beta-PPR RA7050 is steel grey similar to RAL7042.In general Beta-PPR RA7050-GN is intended to be used in applications for plumbing and heating, such as in-house hot and cold water pipes and fittings, floor and wall heating systems and radiator connections. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Surface Resistance
- CTE, linear 20°C
- Thermal Conductivity
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Head Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|