Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes
Subcategory: Polypropylene; Thermoplastic
Material Notes: BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according to EN 1852-1/A1 and is a PP-HM (polypropylene high modulus) material.BorECO BA222E is recommended for solid wall non-pressure piping especially in underground drainage and sewerage and soil and waste applications. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Front Barrel Temperature
- Die Temperature
- Melt Temperature
- Head Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|