Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible crosslinkable pipes. BorPEX HE 2515 is designed for the requirements in DIN 16892/BIN 16887 for hot water pressure pipes, e.g. floor heating, radiator connections and for domestic hot and cold water supply. Documentation is available on request. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength at Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Modulus of Elasticity
- CTE, linear 20°C
- Specific Heat Capacity
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|