Borealis BorPEX™ HE2556 Black High Density Polyethylene Powder for Crosslinked Pipes
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: BorPEX HE2556 is a black, high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for peroxide crosslinking. Well dispersed carbon black give outstanding UV resistance. Long term stability is ensured by an optimized stabilization system. Crosslinked pipes made from BorPEX HE2556 are recommended for drinking water and industrial applications. Information provided by the Manufacturer.
| Available Properties |
- Density
- Carbon Black Loading
- Melt Flow
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|