Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is ensured by an optimized stabilization system. Crosslinked pipes made from BorPEX HE2557 are recommended for natural gas and industrial applications. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|