Borealis Borcell™ HE1345 High Density Polyethylene Compound for Cellular Insulation of Telephone Singles
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Borcell HE1345 is a high molecular weight, high-density polyethylene (HDPE) insulation compound containing an industry approved non plate-out chemical blowing agent and contains the required levels and types of primary antioxidant and metal deactivator to satisfy stringent standards for product longevity. It is capable of 50 percent Borcell HE1345 is designed for the production of foam or foam-skin insulations in either air-core or grease filled copper cable constructions. Information provided by the Manufacturer.
| Available Properties |
- Density
- Oxidative Induction Time (OIT)
- Tensile Strength @ Yield
- Elongation at Break
- Dielectric Constant
- Dissipation Factor, Low Frequency
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|