Borealis Borcell™ LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: Borcell LE1120 is a low density polyethylene intended for the insulation of coaxial and radio frequency communication cables.. It contains no additives and is designed to give the lowest possible attenuation by the selection of "electrically clean" feedstock. Strict cleanliness requirements are applied in production and materials handling. Borcell LE1120 is designed to be used as insulation for radio frequency cables having extra high demand on low attenuation at high frequencies. By blending weight a suitable stabilized HDPE component prior to the extrusion, in an optimum ratio for each insulation thickness, the lowest possible attenuation can be achieved. A small amount of HE1102 is recommended as nucleating agent. Using optimized-processing conditions an expansion above 80% can be expected. Information provided by the Manufacturer.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Yield
- Dielectric Constant
- Dissipation Factor, Low Frequency
- Middle Barrel Temperature
- Front Barrel Temperature
- Die Temperature
- Head Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|