Borealis Borclear™ RD738CF Propylene Alpha Olefin Copolymer for Cast Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Borclear RD738CF is a slip and antiblock formulation propylene alpha olefin copolymer resin. It is suitable for the manufacturing of unoriented film on chill roll process.Borclear RD738CF is suitable for various high quality film applications including food packaging, high quality stationery, lamination film, textile packaging, and sealing layer in coex-structures. Information provided by the Manufacturer.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Flexural Modulus
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Impact Test
- Coefficient of Friction
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|