Borealis Borcoat™ BB108E-1199 White Polypropylene Block Copolymer for Steel Pipe Coating

 

Subcategory: Polypropylene; Thermoplastic

Material Notes:
Borcoat BB108E-1199, a ready made white compound, is a highly molecular weight, low melt flow polypropylene block copolymer. As a top-coat in three component polypropylene systems, Borcoat BB108E-1199 fulfills the requirements in NFA 49-711, DIN 30678, Shell specification (DEP 31.40.30.31) and Pr EN 10286 when used in combination with Borcoat BB125E or Borcoat BB127E and compatible powder epoxy and applied under sound processing conditions.

Borcoat BB108E-1199 is used in steel pipe coating as a top-coat for three component systems, UV stabilized, highly protected against thermal ageing, and designed for continuous use at high temperatures 110°C on-shore and up to 140°C for very specific off-shore projects.

Information provided by the Manufacturer.

Available Properties
  • Density
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Yield
  • Flexural Modulus
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Notched
  • Vicat Softening Point
  • Front Barrel Temperature
  • Die Temperature
  • Melt Temperature
  • Head Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。